novice

 





 

2.2 The heat resistance of the coating is extremely sensitive to water. In humid environments, heat resistance decreases significantly. The thermal decomposition temperature in the dry environment is 130 ° C, and the thermal decomposition temperature in the humid environment is only 60 ° C, which leads to the limited use environment of chlorinated rubber coating, and the maximum use environment temperature cannot exceed 70 ° C.


 